finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 30016

Material surface finishing problem

        

++++

I am from the metal industry and I am facing problems with the Material surface finishing problems listed below: - Galvanize Iron

1) Black patches with looks like oil stain which is unremovable from the material surface.

2) material discoloration near both edges of the coil
- sometimes the edge surface is brighter than the center portion of the material surface.
- sometimes the edges are darker or black.

3) Intermittent black lines running along the coil surface.

Vin
metal industry - Singapore

Ed. note: Hello, Vin. Our experience here indicates that our readers are usually little inclined toward spending their time to help a stranger who keeps himself anonymous, offering only a nickname and disposable e-mail address. Please give us your full name and what you do, and a little detail about the installation, and I think someone will help you further. Thanks!


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search