Looking for an acid to eat through bolts on a metal structure

++++

I am looking for an effective way to dissolve rusted bolts from an old swingset. I figure if I can use acid to eat through the bolts the dismantling will be easier. Would you recommend Sulfuric Acid, Hydrochloric Acid, or is there an over the counter product that would work better?

Thank you,

Greg Wehking
hobbyist - New Berlin, Wisconsin, USA


++++

A method we are unfamiliar with always seems easier than the one we are familiar with, Greg :-)

But get a hand held grinder; they're cheap these days and will make fast work of this problem. It is terribly unsafe and an unenvironmental shame to attempt dissolving bolts in acid. And don't be unduly influenced by what you see in the movies; what you want to do would take days, not seconds.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


July 29, 2010

The chemical you are thinking of is called THERMITE

david lawry
- san francisco, california, san francisco


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search