I am attempting to figure out a call out for cadmium plating. The call out is as follows "CD 10 FIC". Its on a European blueprint for a aircraft fastener. What is it and where can I obtain information over the web regarding it.

Thanks,

Dave Miller
- Los Angeles, California, USA


++++

Hi Dave,

I had the same problem with the definition, but I have solved it yet.

Cd10 FIC = 10µm Cadmium without finish code
-natural coloring of the chromic finsh-

Please look at the paper of Aerospatiale Aeronautique NSA5414 (Issue J / Date 10.98) Page 4.

Mr. Kaßner
airplane coating centre - Dresden, Germany

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search