Zinc plating for 400 hours of salt spray test

   

++++

I am looking for information on zinc plating that will pass 400 hours of salt spray testing.

Arvind
manufacturer - Hosur, TN, India


++++

Maybe it would be easier to look for salt fog cabinets that allow your current zinc plating to survive for 400 hours :-)

Sorry, Arvind, just a joke based on a discussion last year. Must this be straight zinc or can it be a zinc alloy? Hexavalent chromates permitted? Barrel or rack? What material is the substrate? Please flesh out your inquiry with some detail. Thanks!

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++++

Your requirement of Salt Spray 400 hrs not specified whether white rust or red rust, in any case Zinc Alloy Plating with Iron or Cobalt in alkaline process is very much suitable. Depending upon the requirement of Chromate colour, you have to select the above process. Chromate may be hexavalent or Trivalent. I have got experience in achieving 400 hrs salt spray with the above process.

P. Gurumoorthi
    electroplating process chemicals
Chennai, Tamilnadu, India

++++

I want to meet 400 hrs of salt spray test using a trivalent plating without sealant. Currently we are using hexavalent plating. Has anybody achieved this without a sealant. I am interested to know more about this.

N.Kumaran
- Tamilnadu, India


++++

Arvind,

If you need 400 Hrs I suggest Zinc Iron Alkaline bath Plating followed by Trivalent Light Green Chromate which will exceed the 400 Hrs. The chemistries are available in India from Proprietary makers.

Regards,

Asif Nurie
Atlanta Global

New Delhi, India


++++++

Dear Sir/Madam
Hello
I want to coat(Zn coating) for parts (sheet metal)for up to 24 Hours salt spray test and with smooth surface.
please inform and help me.

Best Regard,

Sadegh Gholipour
- Tehran, Iran


May 30, 2008

I would like to know how long time in each color chrome (blue, yellow and black) for salt spray test in according JIS Z 2371 standard?

Arnupap Siriphan
Owner - Thailand


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search