Multiple colour acid etching on 304 SS

++++

Hi,

I am redesigning an intercom panel which is currently a 3mm thick 304 stainless steel panel, powder coated white, blue paint filled acid etching, with a clear anti-graffiti coating. We are looking to increase the number of colours from just blue, to red and blue. The two colours are mostly separated except one area where they meet. This meeting can be separated by a non-etched area if required. I would appreciate guidance in the best methods to employ to achieve this result. panel size: 200mm x 200mm quantity: approx. 50 units details: ~ speaker, mic and button holes ~ weldstuds on rear.

In appreciation of your time,

Jareth Bone
electronics design - Brisbane, Queensland, Australia


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search