Can you plate titanium

++++

I need to pen plate titanium. Can it be done with standard pen plater? Tried on steel and it plates but it does not seem to work on the titanium

Boyd Lenkersdorf
manufacturing - Palm Beach, Florida, USA


++++

I do not know what "pen" plating is - is it another name for "brush" or "tampon" plating? The problems of plating onto titanium have been widely discussed on this site, so try 4497, 10897, 13254, 13456, 26878 and 27397. As far as I am aware, it is impossible to electroplate titanium onto a substrate from an aqueous solution, but there are some claims that it can be done. I would be interested to know what pen plating is.

Trevor Crichton
R&D practical scientist The Pheasantries - Chesham, U.K.

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search