Latest trends in Dacrotizing process
++++
Hello Sir,
I am a student of BE Production (Pune University India). I would like to know the complete information about the latest trends in Dacrotizing for my Seminar presentation as a part of my Seminar work. Can you send the web addresses of relative sites to this topic ?
Praj [last name deleted for privacy by Editor]Student of Pune University. - Pune, Maharashtra, India
++++
Hi, Praj. I believe that Dacrotizing involves the dip-spin deposition of a zinc-rich paint as an alternative to electroplating, mechanical plating, or galvanizing. Try Metal Coating International as Dacrotizing is their trademark. Good luck.
|
Ted Mooney, P.E. RET finishing.com Brick, New Jersey |
March 22, 2011
Sir,
Please tell me every thing about Dacrotizing. I am about to set up a plant for Dacrotizing. I am new to this field. I need your guidance on this subject. I am interested to know more on the preparing the paints, then the testing procedures to avoid failures.
I hope to get a reply soon.
regards,
MOTOR WORKS - Chennai, TN, India
March 24, 2011
Hi, Raj.
If you have questions about the generic idea of dip-spin coating with zinc-rich paint, you might get multiple ideas about it. But if your inquiry involves Dacrotizing specifically, the only people to help you would be Metal Coating International as it is their product. Good luck.
Regards,
|
Ted Mooney, P.E. RET finishing.com Brick, New Jersey |
January 6, 2012
Hi Sir
I want to set up a Dacrodising plant and require service providers to assist me in this process.
A full set up costs etc.
Thank you
plating - South Africa