Powder Coat plus Silver Nickel

++++

I have some 1008/1010 parts that require a powder coat finish with a silver nickel finish applied to an area that was masked during the powder coat operation. Can the silver nickel application cause the powder to "peel?".

Kathy Hewitt
stamping company -Fraser, Michigan


++++

It's hard to say. On the one hand a plating process is quite aggressive, with alkaline cleaners, acids, etc. On the other, this process of plating the uncoated areas of powder coated parts is certainly done.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search