Been reading some of the stuff on the finishing.com website and it is a world of information,

We have a problem in that we need to achieve a high quality finish,

We have considered using Vibro finishing but our parts are made from aluminium 6063 35 mm tubing and are 2 foot by 2 foot by 35 mm, so the Vibro machine is quite big, and we will only get 2 parts in the machine per run.

So we are considering a chemical process of cleaning and brightening, Where we could do a batch of by dipping the parts in a process of several Tanks.

However the Chemicals that are used for best results is Phosphoric, Sulphuric and Nitric Acids. Heated and cooled to very controlled temperatures making the Process dangerous require Scrubbers for the Toxic Fumes.

We are located in UK and there is no current suppliers for this Process.

Currently these parts are scrubbed by hand with Scotching Pads and Wire Brushed at the areas where suit deposits are from welding, this gives a brushed matte finish but we wanted to improve this to a brighter finish.

As we wanted to integrate this process in house but if possible avoid the use of the Lethal Chemicals and a process that require considerable experience to operate.

However  we have been told that there is chemicals that obviously don't give as bright a finish but don't give off the large quantities of NOX.

Do you know what such chemicals are and who could supply them, as we would prefer to do a process without the Heating of the chemicals.

Regards

Dave
- Northern Ireland


++++

Please look for book The Surface Treatment and Finishing of Aluminum and Its Alloys by S. Wernick, R. Pinner, P.G. Sheasby.

Hadi Khosravi
- Tehran, Iran


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search