Nickel-chrome plating wood (MDF)

++++

I have recently heard of an application involving the nickel/chrome plating of wood, specifically MDF. If anyone has any info about the process I would greatly appreciate it. I live in Toronto Canada.

Thanks,

Matt Dinsmore
fabricator - Toronto, ON, Canada


++++

Hello Matt,

Maybe this is interesting for you: in the past I have carried out a "few" tests to cover the surface of LACQUERED wood with gold, using a wet technique. Adhesion is excellent, and the gold is shining yellow. Unfortunately shortage of money and troubles with my health forced me to stop the tests. There are some reproduceable results. The thickness of the gold layer has been measured and compared to common 231/2 crt. gold leaf: it is 1/4 of that.

Ruud Kooijman
- Venlo, The Netherlands


++++

Hi, Matt, have you tried CVD method? Or salt decomposition method.

Victoria Fink
- Vancouver, BC, Canada


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search