Severe corrosion in a wet steam system

++++

I have a problem in one of economiser. Inlet condition : water (Demin + condensate, pH 6.8, no control on O2). Outlet condition : 60% sat. steam + water at 170 C problem : Severe corrosion at outlet side

PANNALAL CHAKRABORTY
engineer in petroleum refinery - HALDIA , WEST BENGAL, INDIA




February 3, 2012

Q. What is the importance of economiser inlet pressure?

Dinesh R
- Chennai, India

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search