What powder coating thickness for aluminum workstations?

   

+++

I am working in the modular furniture industry, where we use aluminium extrusions for making frames. On those aluminium extrusions we do powder coating . So I would like to enquire about powder coating thickness. These aluminium Extrusions will be assembled and made into the structures of WORKSTATIONS. These workstations are erected within the office premises on the customer end, and they are not exposed to any atmospheric / weather conditions . Hence we require that the coating thickness for these workstations shall be in the range of 40 to 60 microns or 60 to 80 microns. PLEASE ADVICE FOR COATING THICKNESS RANGE OF STRUCTURES.

KISHOR PATIL
Quality Engineer - NAVI MUMBAI, MAHARASHTRA, INDIA


+++

Hi !

In my opinion, the thickness should be between 40 to 60 , for the best results.


Atul Bhide
jobshop / applicator - Mumbai, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search