finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 26080

Reduction and Precipitating of Copper from its salt solutions without using electricity

+++

I am trying to reduce metallic copper from cupric solutions and have tried different reducing agents such as Sulfoxylates, sodium borohydride, Sodium hydrosulphite and THPC but I am looking for more reducing agents because none of these could fulfill my necessities. It must reduce copper at room temperature and in a non toxic environment with high efficiency and the precipitated particles must be very fine. I would be very grateful if you could give me some pieces of information according to your experience and researches.

Best regards,

Mansour
PhD student - leeds, yorkshire, u.k.


++++

to have a fine copper powder you can use Zn,Al ,or H2.in case you are looking for a ultrofine copper why not to try colloidal copper and to destroy the colloid afterwards. for detailed information contact again and I'll submit procedure. good luck


Cair Shishani
aircraft maintenance - Abu Dhabi, United Arab Emirates


+++++++

Dear Sir

I saw a response from Cair Shishani; I would also like to get a procedure for reducing and precipitating copper from its salt solutions without using electricity. He mentioned the use of Zn, Al, H2 and colloidal copper. I am interested in the use of colloidal copper and and hydrogen. I will apprecaite if I can get this information urgently.

Regards

Soco

Soco Mncube
biotech - RSA, Pretoria


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search