Knife sharpener mfgr. needs diamond composite plating [South Africa] 

+++

Diamond plating. I would like to have the one side of a square zinc diecast rod to be plated with D46 Diamond.The surface area of the side that has to be plated is 5 mm x 105 mm. The face is slightly convex. If interested please give quotation for 2000, 4000 and 6000 units.