Highly Reflective / High Temperature Paint

+++

I am looking for a paint that has high reflectivity (like chrome), can operate in temperature environments at ~250 degrees F, and I can spray for my application. Aluminum colored paints are not reflective enough.

Roger Johnson
Mechanical / Aerospace - Cary, North Carolina


+++

You might try a paint with vacuum metallized aluminum pigment in lieu of a standard aluminum flake. Most industrial paint companies should know what you are asking for when you contact them. The vacuum metallized pigment can provide highly reflective properties when incorporated into the right binder for the application. Good luck.

Michael A. Koons
industrial coatings - Willoughby, Ohio


+++++

I am searching for a paint which is highly reflective with reflectivity(0.95-0.99) compatible over a aluminum surface. It is for industrial application.
Give with company details.

S.Annie
- Banglore, Karnataka, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search