Need a coating for copper pipe to prevent weathering and verdigris

 

+++

Our exterior deck has railing balisters made with 1/2 inch steel rebar inserted into 1/2 inch copper plumbing pipe. We would like to clean the copper and then coat them to prevent them from weathering. They are only slightly discolored at the moment. The problem is that we aren't sure how or what to use to accomplish this. Our original plan was to let them weather, but we have had so many compliments about the unweathered copper that we have changed our minds.

W. Martin
hobbyist - Silverdale, Washington, USA


+++++

I installed half inch copper pipe for ballusters on my new deck and am curious what, if anything, you've done to keep the pipe looking like "day one".

Ted Dedden
- University Place WA USA


+++++

A lacquer with benzotriazole corrosion inhibitor sounds like the best bet.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search