Letter 25068
Is it possible to etch indium w/o etching aluminum?
+++
application = 10-20um indium bumps on aluminum IC pads.
problem = reworking indium bumps.
Questions: Is it possible to etch indium w/o etching aluminum? or Is it possible to repair IC pads if damaged (not necessarily with the same metal)?
Stephen Gabelich
electonics - El Segundo, California, USA
Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.