Letter 25065

Plating copper buss bars  

+++

I am a process engineer for a company that produces energy controls and surge protection devices. We are designing a series of copper buss bars to be used in one of our applications. The copper bar is 0.375" wide x 0.125" thickness consisting of various lengths. I am looking for a relatively inexpensive method for protecting these from corrosion. Our plating vendor suggested yellow chromate while a fellow engineer suggested bright dipping them. Are there any other reasonable methods I should look into?

Domnic Grujic
Engery controls, surge protection devices - Chicago, Illinois, USA


+++

BRIGHT DIPS PROVIDE VERY LITTLE CORROSION PROTECTION. YELLOW CHROMATE IS VERY GOOD. SOME NICKEL PLATE COPPER BUSS BARS FOR CORROSION PROTECTION.

Don Baudrand
Don Baudrand, Consultant
 
Poulsbo, Washington


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com