Water treatment with CN

     

+++

Which is the ideal treatment for an effluent of brass/copper bath with CN (NaCN, CuCN, Zn(CN)2? As I can eliminate the CN and precipitate the metallics ions?

Diogo Cavalcanti
Home Hardware - Caxias do Sul, RS, Brazil


The ideal treatment always depends on the circumstances, Diogo, but the most comon treatment is 2-stage alkaline chlorination using either hypochlorite or chlorine gas and sodium hydroxide.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search