finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 25020

What is NH35?

+++

What is NH35, its now being used on thixomolded magnesium before powder coating. Also why is it required.

Dave Burrows
- Colorado Springs, CO, USA


+++

NH35 is a type of chromate conversion coating used for magnesium die castings. It was developed by Norsk Hydro as a pretreatment for subsequent painting. It provides for better adhesion, as well as enhanced corrosion resistance. None of the chrome-free pretreatments (Alodine 5200, etc.) have been able to meet the same corrosion performance that NH35 provides.

Toby Padfield
Automotive module supplier - Michigan

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search