finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 25002

Speed of deposition in brass bath

+++

Which are the conditions of work of a brass bath to get a good speed of deposition in brass bath high layer?

Diogo Cavalcanti
Home Hardware - Caxias do Sul, RS, Brasil


+++

Hi. The single thing that must be done to increase the speed, according to Faraday's Law, is to increase the current density. But how to achieve this, while avoiding consequent problems like burning, is difficult to discuss in the abstract. Are you using a cyanide or non-cyanide brass plating bath, Diogo?

You might be interested in Brenner's "Electrodeposition of Alloys".

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search