HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 24116
Pulse plated silver
+++
Hi,
We are a Finish plating shop. One of our services is to silver plate rf-filter bodies. Normally we use inert anodes to have silver about 6µm into deep holes. Now we have a bit too difficult filter body and I am planning to use pulse plating to get desired thickness.
The base material is diecast aluminium and electroless nickel
10µm on it.
My question:
Does anyone have detailed information how to start or where could I have a copy of article (from AESF): Title: "Optimization of Throwing Power in Pulse Reversal Plating from a Silver Cyanide Solution" Authors: P. Leisner, P.T. Tang & G. Bech-Nielsen Reference: AESF SUR/FIN'94, Indianapolis (1994)
Thank you and best regards,
Petri Helin- Kellokoski, Tuusula, Finland
+++
Hi, Petri. The article will be available from www.namf.org, although you may need to buy the proceedings of the whole session rather than just the single paper. Good luck.
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |