HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 24109
Is fusion bonded epoxy coating best for very large item
+++
Specifically we have an application, as below:
Size of item is 2165 mm x 1500 mm x 1500 mm.
Basket Strainer, made in Ductile Iron, GGG 50.
FBE 300 microns is specified.
Is this feasible? If YES, will it be a "good" coating? OR do you recommend some other method of coating?
Regards Govindan
Govindan Menonsuppliers of engineering spares - Dubai, United Arab Emirates