Can anyone recommend a supplier of dry film
lubricant materials per MIL-L-46010 for independant job shop
applicators other than E/M Lubricants?
-
Try Acheson Colloids,
Port Huron, MI (Manufacturers of Molydenum, graphite, PTFE dry film
lubes) We use Emralon (PTFE) and Molydag with excellent results.
Whitford (Frazer, PA) makes Xylan, a PTFE lube we've had good success
with.
Dow Corning makes a Moly coating.
Dupont also markets their own Teflon coatings.
Good luck,
Mike
Michel Moninger
- Sarasota, FL
____
Ed. note: This inquiry was answered with 5 alternatives given. The
inquirer's need was met long ago, so we will not be adding to this
letter. If you have any questions about dry film lubricants, or any
other metal finishing question or need, please see
www.finishing.com/Letters.
Dear Reader:
Sorry, but this particular Commercial Inquiry / RFQ is outdated.
- Please feel free to:
- Post a Question or Inquiry of your own,
-
- View current RFQs at
- "Seeking Jobshop Services"
- or
- "Seeking Products or Services for Finishing Shops" or
-
- View current technical inquiries on the
- "Hotline - Letters page".
 |
|