Electrodeposition of Sb-Se thin films

+++

I am doing electrodeposition of Sb-Se thin films over ITO substrates. But the same thing cannot be repeated using stainless steel substrates. I don't what would be the reason. Will adherence play a role? Some times I get the films coated with graphite which I have used as anode. Tell me your suggestions.

A. CELESTINA
Research student - COIMBATORE, TAMIL NADU, INDIA


October 17, 2009

Hi, A. Your inquiry is a bit brief for me to understand, but electrodeposition with good adhesion onto stainless steel -- which is a very passive substrate -- requires starting with a Wood's Nickel Strike. Detailed info can be found in Jack Dini's "Electrodeposition". Good luck.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search