October 17, 2009 Hi, Zoe. There is a nitric acid spot test for gold; for small users it is available as simple gold test kits ==> But there is probably no legal requirement for any particular thickness, and the actual thickness is probably only about 20 millionths of an inch -- which means there is no real monetary value associated with gold plating. Regards,
|
|
|