Electropolish recipe for 420 grade stainless steel

+++

We have lost our recipes for our electropolisher. Can someone help me with some recipes for 316 grade stainless 420 grade stainless.

Many thanks,

BOB LYE
SURGICAL INSTRUMENT MANUFACTURER - SYDNEY, NSW, AUSTRALIA


October 17, 2009

Hi, Bob. There are many many different recipes, most based on sulphuric acid or a mix of phosphoric and sulphuric acid. The Electroplating Engineering Handbook has an excellent chapter on electropolishing, and includes some recipes you can try.

If you need qualified technical assistance you might contact Metal Coating Process Corporation, which specializes in electropolishing and conducts training schools. Good luck.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search