Chrome look finish for aluminum door handles
+++
I am looking for an appropriate finish to use on a machined aluminum (exterior) door handle. Desire is for shiny "chrome" look. (Anodized and polished aluminum is too dull.)
Part is fully exposed to the environment and gets a fair amount of abuse, so the finish needs to be very durable and adhere well to the part. It also must be to some process that can be certified (i.e. mil-spec...)
Gary PoelmaDesign and manufacture airplanes - Duluth, Minnesota
+++
Fully bright Electroless Nickel alone or with an underplate (either copper or high phos EN). Most commercial and policemen firearms use it nowadays instead of traditional nickel chrome. It looks shiny and is corrosion and wear resistant.
Guillermo MarrufoMonterrey, NL, Mexico