My stepdad is a welder. He was using
Ospho. My Mom was helping
him by apparently sanding or grinding it off the metal it was sprayed
on. As a result she is now very ill, this according to my stepdad.
I'm not for sure if he telling me, my family, or the doctors the
truth or not. The doctors can't say for sure what it is, or isn't
that's causing the trouble. I'm hoping that you could tell me where I
can find info on this chemical, and if you have heard of anyone else
who has become ill using this product.
Kelley K 
- Robertsdale, Alabama
December 27, 2008
A link to the MSDS is at the bottom of this post; the major threat
would appear to be lung damage from the acid if proper breathing
protection wasn't used. Medically this translates into difficultly
breathing and possible pneumonia.
Her illness may have an entirely different cause--the material and
her illness could be coincidental, so make sure that her doctor
checks for any illness, poisoning or such which has similar
symptoms.
Contact the manufacturer or distributor for an MDS. This will list
the chemicals involved and their potential effects.
You can also check with your poison control center.
"SKYCO OSPHO: a balanced formula of
Phosphoric, Dichromate, Wetting Agents and Extenders . . . compounded
exclusively by the Skybryte Company since 1947"
Questions Not Answered Here Call Factory Direct at:
216-771-1590
Chemical
OSPHO is a balanced formula of Phosphoric acid, Sodium Dichromate,
Surfactants, and Extenders.
Physical
Boiling Point 240 degrees F Specific Gravity. 1.22 + .04 Average %
Nonvolatile = 37.6% + / -0.5%
Soluble in Water Color. Green Liquid Odor. Typical Acidic
Spills Neutralize with basic material, flush with plenty of
water.
Respiratory Use adequate ventilation in confined areas, skin and eye
protection should be used.
Fire Data No hazard
Decomposition Products Oxides of phosphorus
Health Hazards Irritant to eyes and mucous membranes. In case of
external contact, flush with cool water. If swallowed, give 1 or 2
glasses of water or milk and call physician.
KEEP OUT OF REACH OF CHILDREN
Reactivity Can react with various metals to generate hydrogen gas,
which could form an explosive concentration in confined spaces. Use