Inconsistency in zinc-nickel finish

+++

I have received sample bolts from suppliers with zinc-nickel alloy and a clear trichromate coating. These are the same bolt but the bolt from one supplier is a bright nickel and from the other supplier is a matt silver finish. Both pass the 240 SS requirements. Why the difference in appearance?

John Fraim
- Scottsville, KY, United States


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search