Wanted glue for ss to ss bonding

+++

We are one of the leading manufacturers of Elevators in India. We manufacture SS door panels for our elevators . We are looking for some adhesive / glue which will bond SS to SS or Stainless steel to MS . please recommend by return mail With Best Regards S Datta

s datta
- mumbai, maharashtra, india


+++

That isn't the way it is usually done, Mr. Datta. Rather, sheets of stainless steel are autoclave bonded to sheets of steel (or lower grade stainless) at the steel mill and then rolled down to the desired thickness.
pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey



----
Readers: This site is made available for camaraderie & technical info exchange by our supporting advertisers, and they will contact the inquirer privately regarding their commercial needs. Please offer comments on any technical issues, but not sourcing suggestions or testimonials. Thanks!


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search