Scratched Bead Blasted Architectural Stainless Steel - HELP?? 

+++

Is there any way to refinish bead blasted architectural stainless steel in place w/out re-blasting?

Jason Young
construction company - Tulsa, Oklahoma


+++

Sounds like trying to take a shower without getting wet. Sorry.

Jon Quirt
- Minneapolis, MN


+++

Not really. The only way to achieve the same texture is via blasting. You can change the texture of the whole piece using other mechanical methods and there maybe chemical processes to clean the whole piece, but each of these methods requires good controls especially the larger the size of the part which you did not mention.

AF Kenton
Nova Finishing Systems Inc.

Huntingdon Valley, PA


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com