Chrome plating bicycle frame

   

+++

I am looking for a place in central Arkansas that has the facilities to chrome plate a bicycle frame. Any help will be appreciated. Thanks.

Jason W [last name deleted for privacy by Editor]
- Beebe, Arkansas, USA
  ^- Sorry! This RFQ is outdated -^


March 20, 2011

Hi, Jason.

In these post Erin Brockovich days, chrome plating shops aren't as common as they once were; and some automated shops are set up only for high volume production runs. But see the banner at the top of the page for some shops, and search our Jobshops Directory for more. Good luck!

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search