HOME
FAQs
BOOKS
JOBS: Help Wanted
Suggestions
you are here: Hotline/Forum =>
Letter 22061
Glass Phenolic Composite Mold Part Coating
+++
Here in JERCN we research about some composites such as glass-phenolice by some process as filament winding, pressure molding,etc. I want to know what is the effect of using from hard chrome (Cr) on the mold parts and what is information about it?
N.Gholizadeh
- Tehran, Iran
Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.
If you are seeking a product or service related to metal finishing, please check these Directories: