Conductive paint for rf shielding

+++

We are designing a vhf radio. For rf shielding we use milled aluminum enclosures, but the weight is a constraint . What conductive paint should I use on what plastic to achieve similar rf shielding?

D.K.Sunil
- Hyderabad, Andhra Pradesh, India


+++

There is a lot of exciting stuff going on with Inherently Conducting Polymers (ICP's) and these may meet your needs. It is possible to get polymers that have conductances ranging between a total insulator and that of some metals.

Trevor Crichton
R&D practical scientist The Pheasantries - Chesham, U.K.

++++

I am also looking for a conductive paint for a plastic enclosure to supress emi and emc.

Ashwin Khemani
- Bangalore, India


June 19, 2008

I would like to know about conductive paints that can be applied over Mild steel sheet or Plastic sheet which will give simialr performances (lesser is also ok) of aluminium sheets for RF applications

Senthil Kumaran
Designer - Chennai, India


April 1, 2010

Y-shield HSF54 is pretty good, it offers consistent attenuation and resistivity than most paints I've come across if you need to consider weight.

NOALE Chris
- Midwest, Missouri


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search