MIL-C-5541 Class 3
+++
Dear Sir, we are currently looking for Mil-C-5541 [link is to spec at TechStreet] Class 3 Type. I only can find the MIL specification informaiton, but no cross-refernce to any product. May it be possible to send a cross reference list between MIL-C-5541 Class 3 to the common used product. Within your information (Questions and Answers) I only found the IRIDITE, but there should be another type of coating being reference to.
Thank you for your help.
Best Regards,
Weidenbrueck, Geraldairline - Cologne NRW, GERMANY
+++
Hello, Mr. Weidenbrueck
There is a separate spec, the "Qualified Products List", QPL-81706 [link is to spec at TechStreet] which lists the products which are qualified to be used in Mil-C-5541 chromate conversion coating.
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |