Control methods

+++

In the framework of my internship, I am doing a benchmarking about electroplating bath control. What kind of on-line control methods do exist nowadays ?

Kévin Menguelti
- maizieres les metz, Lorraine, France

+++

That's a pretty broad question. Remember that temperature has been controlled by on-line control for decades and is virtually universal. Frankly, not much else is controlled by on-line control. Certainly a number of automatic controllers were sold for electroless copper solutions, and there have been a few automatic titration systems installed for other plating solutions, but it's still almost universally done manually.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


+++

Thanks for your response Ted, I would like more specifics indications about automatic titration systems for plating solutions(short method principle and instrumentation to measure components contents of electroplating baths)please. Or where can I find these informations?

Thanks in advance.

Kévin Menguelti
- Maizières-lès-Metz, Lorraine, France

+++

A general introduction can be found in "Control of Plating Chemistry by Voltammetric Techniques", by Marc L. Rothstein, Plating & Surface Finishing, Nov. 1984. I'm confident that the MFIS-CDROM could find you several other literature citations.

In my personal experience, though, this idea just never really took off and there seems to be less interest today than there was in the 1980's when several suppliers were promoting it. I would suggest using a search engine with terms like "on-line analysis plating", and getting some current literature from those companies offering it.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


+++

Dear Ted, Thank you for your answer which helped me in my research.

Best Regards. Kev. (Kiss from Hélène my wife)

Kévin Menguelti
- Maizières-lès-Metz, Lorraine, France

+++

You're certainly welcome Kev. I think EG&G Princeton Applied Research may still be involved in this, but I don't know any other companies that are. Can I collect the kiss in person instead of virtually? :-)

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search