Anodizing pitting problem

+++

The problem is material anodizing is pitting. Not all the time mind you. It has been stated that when both the welder (high frequency) and the rectifier are in use the problem occurs. But not all the time. Does this have to do with shielding or lack of. The solution. Or something else.

Richard Ilnisky
- Saskatoon, Saskatchewan, Canada


+++

I don't think enough info has been provided for anybody to do anything but take a wild guess. But if the problem happens while welding, and not at any other time, it certainly does sound like the electronic noise of the welder may be upsetting the SCRs on the rectifier.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search