EDP Process
+++
I am looking for an explanation for EDP Process (some kind of electrical coating process) for the alumunium material. What is the differences between this process with powder coating.
Sony FirdausPT. Dharma Polimetal - Jakarta, Jakarta, Indonesia
+++
Electro Deposited Paint also called Electrocoat is probably what you are looking for. The chemicals are mixed in a water bath.
The component is made anodic in the anodic process and cathode in the cathodic protess.
On passage of current the coating is deposited on the component. It is cured in an oven.
|
Gurvin Singh Coatec India - Mohali, Punjab, India |