Need gold plated glass  

+++

I am looking for 1mm thick soda glass that has a thin gold film on one side. It needs to be slightly conductive but still pass visible light. I am thinking of the face masks I remember the Apollo astronauts wearing. The glass will be cut to 25mm x 75mm size for use on medical instruments.

Chuck Lemme
- Tucson, AZ, USA


+++

Direct gold adhesion to glass may be a probelm. Also, gold becomes opaque very quickly at about 100 A thickness. What transparency are you expecting, 50%, 30% ? Do you need a transparent conductive film or must have gold?

Mandar Sunthankar
- Fort Collins, CO


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
I want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com