Finding the rms value for the entire object

+++

I am doing the project n measurement of surface roughness using image processing. Can anybody give me idea of how to measure the rms value by image processing techinque. If anybody knows please send me reply to me, it will be very helpful to me.

Vijayanand
- Coimbatore, Tamil Nadu, India


+++

To my knowledge there is no over all imaging rms system for the whole part. What is normal is to take readings randomly on a part and to use the average of at least 3 to 5 readings, but part size is also a factor. More readings maybe required.

AF Kenton
Huntingdon Valley, Pennsylvania

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search