Solder plating of nickel plated leadframe
+++
We're having problem in solder plating a Nickel base leadframe, blister & peel. Thus anyone know how to make a Cathodic Degreaser. Currently we're on Anodic Degreaser.
Joel M. SupnetFastech Synergy - Laguna, Cabuyao, Philippines
+++
There might be a non-sequitur there, Mr. Supnet.
|