White Rust and Discoloration on Zinc Plated Parts

+++

We are having a problem with "White Rus" and discoloration on some CRS plated parts after the parts are powder coated. The customer specification for plating is as follows: FINISH: ZINC PLATE PER ASTM B-633 [link is to spec at TechStreet]-85, TYPE II Fe/Zn 8, COLOR YELLOW CHROMATE The parts are then powder coated. What can we do to prevent this from happening and allow for the maintenance of the shiny Gold Zinc appearance?

Regards,

Dan Chew
- Round Rock, Texas


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search