We are looking for suppliers of P.P.sheets to be used for chrome plating baths or suppliers of plating baths made from pp-sheets.

Mohammad-Reza Mirshamsi
Shibeh Co. - Tehran, Iran


+++

One of us is misunderstanding something. PP is not satisfactory for chrome plating baths.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


+++

Hi Mohammad,

Nbg. Don't! What Ted says is correct. Go and see the archives # 8169, please.

Where PP will initially fail is at the welds. Who ever suggested PP for chrome is leading you up the garden path!

Just go on the internet and hit your favourite site ... with words like 'what materials for chrome' or 'plastics for chrome' and you should get some good answers.

Freeman Newton - White Rock, British Columbia, Canada
Ed. note:
Please keep Freeman in your thoughts
& prayers.


Message from Freeman, Dec. 2010


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search