Letter 20101 Brushed Chrome Finish [China]+++ We have a request for a metal ( cold rolled steel) ficture to have a BRUSHED CHROME finish. How is this done and is there an additional cost over bright chrome plating? Thank you, Bob Mendelow
+++ You will need to brush the part before plating. After brushing, just perform a normal plating, you will have a brushed finish. Compare to the polished component, there should not be any difference on the cost. Xiao Liu