Nickel on chrome & zirconium

--

We need help finding plating processes that will deposit nickel on zirconium and nickel on pure chromium substraits.

Thank you.

Tom Dudenhoeffer
Klein Plating Works - Erie, Pennsylvania


ASM's Metals Handbook Volume 5: Surface Engineering has some useful stuff on preparing refractory and other difficult-to-plate metals.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search