Magnetic Shielding Coatings

--

I am looking for a spray-on coating for plastics (ABS) that will effectively shield low frequency (60-1200 Hz) magnetic fields. Field strength reduction desired is about 25dB.

Chris Wiegel
engineering - Woodinville, Washington


--

Acheson Colloids and Spraylat both make EMI/RFI coatings that would be suitable. We've had good results with the Acheson products in particular, but use both.

Michel Moninger
- Sarasota, Florida


-

I kindly request more detail about "Magnetic Shielding Coating".

Dr. Nurettin UMURKAN -
yildiz Technical University - Istanbul - TURKEY


-

Need Magnetic Shielding Coating I am looking for a spray-on coating for plastics (ABS) that will effectively shield low frequency (50 Hz) magnetic fields. Field strength reduction desired is about 0.5G.

Tam Chi Lam
technical services - Hong Kong


-

We are a skirting duct (electrical raceway) manufacturer and we are searching for information regarding the use of polymer (plastic) ducts which house adjacent cable runs of both 240 volt power and Cat5 data cable. There is not enough evidence to suggest UTP cannot be used with high speed data transmission. Perhaps a magnetic shielding coating will do the job? Does anyone else have results of any research?

Colin Wynn
- Brisbane, Australia


-

I'm looking for a coating that can be applied to aluminum. The more magnetic shielding the better!

Milton Sigelmann
- Seattle, Washington


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search