Letter 2092
Zinc Dichromate
--
Could anyone please tell me what the general process is for "Zinc
Dichromate"? It's a ASTM
B-633 [link is to spec at TechStreet], SC3, Type II Colored
Chromate Conversion Coating as my client stated on the drawing. I'm
trying to explain this to my Chinese vendor. It's been a while since
I learned this stuff in college. I barely remember this is different
from Zinc plating because it's rather a chemical process.
Any help will be greatly appreciated.
Feng, Jack
- LA, CA
--
This is zinc plating for service condition 3, followed by a type
II chromate conversion coating. The thing to do, Jack, is to get
yourself and your Chinese vendor each a copy of ASTM specification
B633 by following the hotlink.
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|
-
-
 |