i need to match two components in color/finish, one is made of brass the other of aluminum, my problem is that I can anodize the aluminum anyone of several different colors but the problem is that I can't seem to find a way to have the brass any other way than brass, nickel plated both bright silver or dull black. Is there any other way? if not how do I preserve the bright brass finish for 2 years in an inside environment?

thank you for your help

aldo laghi
- clearwater fl


--

Dear Aldo ,

Have you thought of Gold Anodize the Aluminium , and Gold plating the Brass part after Bright Nickel plating , many shops will be able to match the colors for you of if you want to do it yourself contact "Technic Inc" who will be only too willing to help

Best Regards


John Tenison - Woods
- Victoria Australia


--

We have had good success painting both brass and aluminum components. Perhaps a paint process for both would allow the best match possible.

Michel Moninger
- Sarasota, Florida


--

Hello I,m responding to your website concerning the matter of brass-plating. I,m in the process of plating chess figures, made of lead, could you recommend a suitable solution mix, as I,m finding control of colour difficult. I would also like a recommendation for tank control ie.. material and size.. Thank you

Nigel Hutton
- San Jose


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search