Electroplating of iron deposits

--

Does anybody electroplate iron deposits?

Derek Vanek
SIFCO Applied Surface Concepts

Independence, Ohio


--

Dear Mr. Derek Vanek

I have some experience of ductile Iron plating. We plate tips of soldering iron tips with iron. The deposits are subjected to high temperature stresses and stress due to differrential expansion. At present the job is being done on a lab scale. The deposits are quite successful and users are happy. The same technique should be upgradable for bigger jobs.

Y.V.Deval
- Pune, Maharashtra , India


--

Yes. Currently the only application I have come across is for the plating of soldering iron tips. The iron is plated over copper to enhance the heat "holding" capability of the tip.

At one time, iron plating was very popular for electroforming applications, but with the advent of sulfamate nickel plating, iron was phased out.

Richard Zuendt
- Garfield, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search